Stainless 309 is an austenitic chromium nickel stainless steel and offers a better corrosion resistance than the type 304 because of higher percentages of nickel and chromium. Suitable for parts requiring both corrosion and heat resistance and oxidation resistance up to 2000 °F. Strength at elevated temperatures is similar to that of 18-8 Stainless Steels. […]
330 is an austenitic nickel-iron-chromium alloy metled as AOD melt type. This grade is comprised of approximately 36% nickel giving it excellent high temperature oxidation resistance up to 2200oF. 330 stainless remains fully austenitic at all temperatures and is not subject to embrittlement from sigma formation. It has a solid solution composition and is not […]
Stainless steel 310 is a medium carbon austenitic stainless steel, for high temperature applications such as furnace parts and heat treatment equipment. It is used at temperatures up to 1150°C in continuous service, and 1035°C in intermittent service. Its high chromium and nickel contents provide comparable corrosion resistance, superior resistance to oxidation and the retention of a larger […]
Stainless 317 is an austenitic chromium-nickel stainless steel with excellent corrosion resistance. (317 is a modified version of 316). Its high Molybdenum content enhances the grade’s superior pitting resistance. It is the most corrosion resistant of the 300 Series alloys and possesses the highest tensile and creep strength properties at elevated temperatures.
Alloy 321 (UNS S32100) contains increased titanium for improved strength and heat resistance, making it ideal for applications range of 800 – 1500°F (427 – 816°C). It has excellent resistance to intergranular corrosion. A popular aircraft alloy.
Alloy 355 is a chromium-nickel-molybdenum stainless steel . Alloy 355 may have an austenitic structure and formability similar to other austenitic stainless steels or a martensitic structure and high strength comparable to other martensitic stainless steels depending on the heat treatment. High strengths may be also be attained by cold working.
Type 403 stainless is a corrosion and heat resistant 12% Cr martensitic alloy, very similar to stainless type 410, with the exception of a slightly lower maximum silicon content and a slightly lower maximum chromium content. Good levels of strength, toughness and ductility may be obtained with this alloy.
Stainless steel 410 is a basic martensitic grade which contains 11.5% chromium, offering both exceptional wear and corrosion resistance. 410 is generally used for applications which involve mild corrosion, high strength, and heat resistance.
Greek Ascoloy is a hardenable chromium-nickel-tungsten martensitic alloy. This alloy is an extremely deep hardening grade used for application where high resistance to tempering and stress-corrosion cracking are desired. It also has a superior creep strength, resistance to tempering with the properties of the standard chromium grades of stainless steel.
Stainless 422 is a hardenable, martensitic stainless steel with better strength at higher temperatures as high as 1200 F. It is capable of being heat treated to various high strength levels.
Stainless steel 430 is a ferritic, straight chromium, non-hardenable grade, combining good corrosion resistance and formability characteristics with useful mechanical properties. Its ability to resist nitric acid attack permits its use in specific chemical applications but automotive trim and appliance components represents its largest fields of application. Alloy 430 has poor weldability compared to most […]
431 stainless steel is a martensitic stainless steel that is AOD melted. This alloy offers the best corrosion resistance of the conventional martensitic stainless grades. This grade is often used in the aerospace industry as fittings and boltings requiring high yield strength. Stainless 431 also has the best corrosion resistance to marine atmospheres, also resists attack […]